Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier

Product Details
Customization: Available
Standard: GB
Application: Loader, Construction Machinery, Metallurgical Machinery, Cement Plant, Mining Machine, Thermal Power Plant, Coal Yard
Still deciding? Get samples of US$ 9/kg
Request Sample
Manufacturer/Factory & Trading Company

360° Virtual Tour

Diamond Member Since 2019

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

to see all verified strength labels (24)
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
  • Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier
Find Similar Products

Basic Info.

Model NO.
HC
Material
Aluminum
Type
Wear Resistant Ceramic
Color
Grey
Density
2.0g/cm3
Weight Ratio (a:B)
2:1
Operating Time (Min)
10-30
Solidify Time(H)
4
Hardness After Solidify(Shore D)
100.0
Compressive Strength(MPa)
111.0
Tensile Strength(MPa)
26.5
Shear Strength(MPa)
32
Working Temperature
-20--80degree
Packing a
6.67kg/Kits
Packing B
3.33kg/Kits
Packing a+B
10kg/Box
Shelf Life
12months
Store
Cool Dry Place
Transport Package
10kg/Box
Trademark
firstar
Origin
China

Product Description

Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating China Supplier
Ceramic Bead Filled Epoxy, Ceramic Epoxy Coating Supplier

Ultraming's high impact wearing compound is a two-component, rubber-modified epoxy that offers the wear resistance properties of a ceramic filled epoxy along with impact resistance not usually found in epoxy formulations.

With impact resistance superior to ceramic tile, Ultraming's high impact wearing compound is recommended for lining and protecting flumes, troughs, elbows, hoppers, discharge chutes and other processing equipment that is exposed to both abrasion and impact under typical dry surface temperatures of -60 to +200ºC

Ultraming's range of wear-resistant polymer composites offers extreme performance, enabling quarry operators to optimise wear life and keep their operations up and running.

Item

Index

Color

Grey(White Grain)

Density(g/cm3)

2.0

Weight Ratio(A:B)

2:1

Operating time(min)

10~30(can be customized)

Solidify time(h)

 4

Hardness after solidify(ShoreD)GB/T2411-1980

100.0

Compressive strength(Mpa) GB/T1041-1992

111.0

Tensile strength(Mpa) GB/T6329-1996

26.5

Shear strength(Mpa) GB/T7124-1986

32.0

Working temperature(ºC)

-20
~80(Customized for high temperature)

  • High quality alumina reinforcement to withstand heavy abrasion.

  • Advanced surface tolerant chemistry allows for outstanding adhesion and great performance, even when ideal surface preparation is not possible.

  • Ease of application significantly reduces labor and downtime costs.

  • Easily shaped and formed to any metal surface.

  • Rapid cure time

Ceramic reinforced rapid repair compound that repairs and protects all surfaces subject to abrasion, corrosion and erosion:

Chutes, spools, elbows, pumps, tanks, paddles, tiles, agitators, impellors, ducting, screens, screws, valves, nozzles, fans, baffles, launders, cyclones, underpans, manifolds…Anything!

1.On all vertical or overhead applications, tacking welding expanded metal mesh onto the metal substrate is strongly recommended prior to application of Wearing Compound. 2. Clean, dry, and abrade application surface. The more thorough the degree of surface preparation, the better the performance of the application. If possible, it is recommended that the surface be grit blasted to a Near White Metal(SSPC-SP10/NACE No.2) Standard. For less severe applications, roughening the surface with hand tools is suitable.

 

Mixing:

1. Measure 2 parts resin to 1 part hardener by volume or weight on a clean and dry mixing surface and mix together until uniform in color.(If resin and hardener temperatures are 15 ºC/60ºF or below, preheat resin only to about 21ºC/90ºF but not to exceed 37ºC/100ºF) . 2.Immediately after abrasive blasting, rub a thin layer of material onto the surface to "wet" for good adhesion.

 

Operation:

1.Apply fully mixed material to the prepared surface. 2.Initially apply the material in a very thin layer to "wet" out the surface and avoid air entrapment. 3.At 25ºC/77ºF, the working time is 30 minutes. Working and solidify time depend on temperature and mass; the higher the temperature, the larger the mass, the faster the solidifying . 4.Functional cure time is 7 hours at 25ºC/77ºF. 5.CAUTION! Use approved, positive-pressure, supplied-air respirator when welding or torch cutting near cured compound. Use approved self-contained breathing apparatus when burning,welding, or torch cutting indoors near cured compound. Use approved respirator for dusts and mists when grinding or machining cured compound.

DO NOT use open flame on compound. See other cautions on Material Safety Data Sheet. 